SVR 3L

I/ Introduction
*Production materials: 100% latex
*Production process:

II/ Specification
As per ISO 2000:2014 standard
Parameters | SVR3L | Test Methods |
1. Dirt (retained on 45 micron aperture), %wt | 0,03 | ISO 249 |
2. Ash, %wt | 0,50 | ISO 247 |
3. Nitrogen, %wt | 0,60 | ISO 1656 |
4. Volatile Matter, %wt | 0,80 | ISO 248-1 |
5. Initial Wallace plasticity (Po) | 30 | ISO 2007 |
6. Plasticity Retention Index (PRI), % | 60 | ISO 2930 |
7. Lovibond Colour | 6 | ISO 4660 |
8. Mooney Viscosity ML (1+4) ati 100°C | – | ISO 289-1 |

III/ Application
The Po inde x of this rubber is high (Po > 30), so it is very suitable for products that require high elasticity, high wear resistance, high durability such as car tires, belts, cables and wires. ….vv
IV/ Packing and packaging
1. Packaging: SVR 3L rubber is compressed in blocks of 33.33kg/bale and 35kg/bale, commonly packed in PE bags.
2. Packing: Delivery in 20 feet container
– Loose bales:
Weight per bale | Number of bales | Total weight |
33.33 kg | 600 | 20 tons |
35 kg | 600 | 21 tons |
-Pallets: full wooden pallet or shrinkwrapped in PE film, with 36 bags/pallet and 16 pallets/cont.
Weight per bales | Number of bales | Total weight |
33.33kg | 576 | 19.2 tons |
35kg | 576 | 20.16 tons |